Single-mode bend resistant fiber
Make RequestDescription
Features
Characteristics
Intended for:
- application in fiber-optic sensors with small bending diameters of the optical fiber
- application in fiber-optic communication lines when laying optical fiber in splice cassettes
- working wavelength 1550 nm
- minimum bending diameter without increasing optical losses
- small optical losses on working wavelength
Optical Specifications
Attenuation (for 1550 nm wavelength) |
Not more than 0.45 dB/km |
Numerical Aperture |
0.187 |
Cable Cutoff Wavelength (λcc) |
λcc ≤ 1480 nm |
Mode-Field Diameter (MFD) (for 1550 nm wavelength) |
9.1 ± 0.5 µm |
Macrobend Losses
Mandrel Diameter, mm |
Number of Turns |
Wavelength, nm |
Induced Attenuation, dB |
3,5 | 1 | 1550 | 0.03 |
5 | 1 | 1550 | 0.01 |
7 | 1 | 1550 | 0.01 |
Weld losses
Optical losses, dB |
Welding fiber |
Wavelength, nm |
0,425 | SMF-125 |
1550 |
Dimensional characteristics
Glass Geometry: | |
Cladding Diameter |
125.0 ± 0.1 µm |
Core Diameter |
8.3 µm |
Core-clad Concentricity |
≤ 0.8 µm |
Cladding Non-Circularity | ≤ 0.2 % |
Coating Geometry |
|
Coating Diameter |
250 ± 10 µm |
Coating type: Dual layer acrylate
Operating Temperature Range: -60ºC to + 85ºC
All fibers are rewinded with tension ≥ 100 kpsi (0.69 GPa).*
* In case of higher tension proof tests can be done.
Fiber is supplied in spools from 0.5 km.